High ductility blends of PMMA and polycarbonate-siloxane copolymer
US10655001B2 · kind B2 · utility
Assignee
Inventors
Key dates
| Filing date | Oct 22, 2019 |
| Grant date | May 19, 2020 |
| Priority date | — |
| Expiry date | Oct 22, 2039 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC08L2205/035
- WIPO fieldMacromolecular chemistry, polymers
- WIPO sectorChemistry
Abstract
A thermoplastic composition includes: from about 5 wt % to about 70 wt % poly(methyl methacrylate) (PMMA); from about 15 wt % to about 50 wt % of a first poly(carbonate-siloxane) copolymer having a siloxane content of from about 35 wt % to about 45 wt %; and from about 10 wt % to about 45 wt % of a second poly(carbonate-siloxane) copolymer. The second poly(carbonate-siloxane) copolymer has a siloxane content of from about 15 wt % to about 25 wt % or from about 4 wt % to about 8 wt %.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.