Patent · US Active

Method for efficiently preparing doped optical fibre preform and doped optical fibre preform

US10689287B2 · kind B2 · utility

0Cited by
0References
12Claims
0Family size

Assignee

Inventors

Key dates

Filing dateOct 21, 2016
Grant dateJun 23, 2020
Priority date
Expiry dateAug 13, 2037

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY02P40/57
  • WIPO fieldOther special machines
  • WIPO sectorMechanical engineering

Abstract

A method for preparing a doped optical fibre preform includes formulating, a rare earth material or a functional metal material and a co-doping agent into a doping solution, mixing a high-purity quartz powder with the doping solution, drying same at a temperature of 100° C.-150° C. for 12-48 hours, crushing and screening the same to obtain a doped quartz powder; depositing the doped quartz powder onto the surface of a target rod to form a doped core layer; replacing the doped quartz powder with the high-purity quartz powder, and depositing the high-purity quartz powder onto the surface of the doped core layer to form a quartz outer cladding; and removing the target rod, and gradually collapsing the entirety formed from the doped core layer and the quartz outer cladding at a high temperature to obtain the doped optical fibre preform.