Alloy drill and manufacturing method thereof

US10697048B2 · kind B2 · utility

0Cited by
0References
6Claims
0Family size

Assignee

Inventors

Key dates

Filing dateNov 19, 2015
Grant dateJun 30, 2020
Priority date
Expiry dateNov 19, 2035

Classification

  • Technology area (CPC E)Fixed Constructions
  • CPC primaryE21B10/567
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

Disclosed is an alloy drill. Components of the alloy drill are: 14-30 wt % of a binder phase being one or more of Co, Ni, Fe, and Cu; 0.32-9.7 wt % of an additive being one or more of TaC, MoC, Cr3C2, and MnC; and the remainder as a hard phase being WC. In the alloy drill, WC is used as the hard phase to improve its hardness and wear resistance, Cu, Ni, Fe, or Co as the binder phase can improve its anti-corrosion performance and anti-fatigue performance, and TaC, MoC, Cr3C2, or MnC as the additive can further improve its thermal stability and wear resistance. Thus, the alloy drill has superior wear resistance and impact toughness, and also possesses excellent anti-corrosion performance and anti-fatigue performance.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.