Rubber composition including a hydrocarbon resin with a low glass transition temperature

US10808105B2 · kind B2 · utility

10Cited by
29References
41Claims
0Family size

Assignee

Inventors

Key dates

Filing dateJul 7, 2016
Grant dateOct 20, 2020
Priority date
Expiry dateJan 1, 2037

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC08L101/12
  • WIPO fieldMacromolecular chemistry, polymers
  • WIPO sectorChemistry

Abstract

A rubber composition is based on at least one diene elastomer with a glass transition temperature (Tg) of less than −40° C., one reinforcing filler at a content from 60 to 110 parts by weight per hundred parts by weight of elastomer (phr), one vulcanization system and one combination of plasticizers, the said combination of plasticizers comprising more than 10 phr of at least one hydrocarbon resin with a glass transition temperature (Tg) of between −40° C. and 20° C. and at least one supplementary plasticizer selected from plasticizing oils, hydrocarbon resins with a Tg of greater than 20° C. and their mixtures, the total content of plasticizer being within a range extending from 25 to 65 phr, the contents of reinforcing filler and of plasticizer being such that the ratio of the total content of filler to the total content of plasticizer is within a range extending from 1.8 to 2.5.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.