Method for synthesizing polybutylene adipate terephthalate-polylactic acid (PBAT-PLA) copolyester

US10875958B2 · kind B2 · utility

0Cited by
0References
12Claims
0Family size

Assignee

Inventors

Key dates

Filing dateAug 29, 2017
Grant dateDec 29, 2020
Priority date
Expiry dateOct 4, 2037

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC08G63/85
  • WIPO fieldMacromolecular chemistry, polymers
  • WIPO sectorChemistry

Abstract

A method for synthesizing a polybutylene adipate terephthalate-polylactic acid (PBAT-PLA) copolyester, the method including: uniformly blending a first prepolymer PBAT and a second prepolymer PLA to yield a mixture, 0putting the mixture in a vacuum reactor with a vacuum degree of between 5 and 100 pascal, heating the vacuum reactor to a temperature of between 100 and 110° C., and allowing to react for between 0.5 and 1 hr; stepwise increasing the temperature to be between 145 and 155° C. in between 1 and 2 hrs, and allowing to react for between 5 and 10 hrs, to yield a PBAT-PLA copolyester with a weight-average molecular weight of between 100000 and 250000. The method for synthesizing the PBAT-PLA copolyester is eco-friendly, non-toxic and cost-efficient.