Patent · US Active

Continuous methods of making glass ribbon and as-drawn glass articles from the same

US10906831B2 · kind B2 · utility

2Cited by
5References
18Claims
0Family size

Assignee

Inventors

Key dates

Filing dateJun 20, 2019
Grant dateFeb 2, 2021
Priority date
Expiry dateJun 20, 2039

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC03C3/091
  • WIPO fieldOther special machines
  • WIPO sectorMechanical engineering

Abstract

A method for making a glass ribbon that includes: flowing a glass into a caster having a width (Wcast) from about 100 mm to about 5 m and a thickness (t) from about 1 mm to about 500 mm to form an a cast glass; cooling the cast glass in the caster to a viscosity of at least 108 Poise; conveying the cast glass from the caster; drawing the cast glass, the drawing comprising heating the cast glass to an average viscosity of less than 107 Poise and drawing the cast glass into a glass ribbon having a width (Wribbon) that is less than Wcast; and thereafter cooling the glass ribbon to ambient temperature. Further, the cast glass during the cooling, conveying and drawing steps is about 50° C. or higher.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.