Patent · US Active

Lithium conducting ceramic oxide decontamination method

US10923765B2 · kind B2 · utility

0Cited by
0References
16Claims
0Family size

Assignee

Inventors

Key dates

Filing dateDec 31, 2018
Grant dateFeb 16, 2021
Priority date
Expiry dateMay 12, 2039

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY02P70/50
  • WIPO fieldElectrical machinery, apparatus, energy
  • WIPO sectorElectrical engineering

Abstract

A method of decontaminating a lithium conducting ceramic oxide material. The method includes soaking the lithium conducting ceramic oxide material having a first thickness of surface contaminants in a first organic solvent containing an inorganic salt at an inorganic salt concentration to obtain a soaked lithium conducting ceramic oxide material. The method further includes rinsing the soaked lithium conducting ceramic oxide material in a second organic solvent to obtain a decontaminated lithium conducting ceramic oxide material having a second thickness of surface contaminants less than the first thickness of surface contaminants.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.