Magnetic recording medium

US10937457B2 · kind B2 · utility

8Cited by
1References
22Claims
0Family size

Assignee

Inventors

Key dates

Filing dateJul 12, 2019
Grant dateMar 2, 2021
Priority date
Expiry dateJul 12, 2039

Classification

  • Technology area (CPC G)Physics
  • CPC primaryG11B5/851
  • WIPO fieldAudio-visual technology
  • WIPO sectorElectrical engineering

Abstract

There is provided a magnetic recording medium of which an average thickness tT is tT≤5.6 μm, a dimensional change amount Δw in a width direction with respect to a change in tension in a longitudinal direction is 660 ppm/N≤Δw, a squareness ratio in a vertical direction is 65% or more, and a width deformation coefficient b during long-term storage in a case where a long-term storage width change amount Y is defined as Y=blog(t) is −0.06 μm≤b≤0.06 μm.