Adsorbent and method for producing the same
US10960380B2 · kind B2 · utility
0Cited by
2References
16Claims
0Family size
Assignees
Inventors
Key dates
| Filing date | Dec 20, 2016 |
| Grant date | Mar 30, 2021 |
| Priority date | — |
| Expiry date | Jun 30, 2037 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC07K2317/55
- WIPO fieldChemical engineering
- WIPO sectorChemistry
Abstract
An adsorbent, which can be produced by a method in which a particle size, a pore size, a specific surface area or the like can be easily controlled, and is suitable for isolation of biomolecules. The adsorbent contains aggregates of calcium phosphate-based particles, and has an average pore size of 15 to 36 nanometers and a specific surface area of 40 to 90 m2/mL when measurement is carried out by mercury porosimetry.