Patent · US Active

Highly crystalline spherical silk fibroin micro-particles and a process for preparation thereof

US11046737B2 · kind B2 · utility

0Cited by
1References
17Claims
0Family size

Assignee

Inventors

Key dates

Filing dateJan 6, 2016
Grant dateJun 29, 2021
Priority date
Expiry dateJan 6, 2036

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC07B2200/13
  • WIPO fieldPharmaceuticals
  • WIPO sectorChemistry

Abstract

The present invention provides silk fibroin micro-particles having a high crystallinity index (1.3-1.5) and low sphericity index (≤0.01) and a process for the preparation thereof. The high crystallinity index confers longer degradation periods to the instant silk fibroin micro-particles, therefore facilitating their use in biomedical applications.