Abstract

This invention provides a manufacturing method for an optical fiber. In this invention, when the core layer loose body and the cladding layer loose body are deposited, the oxyhydrogen flame is used make a temperature of an interface between the core layer and the cladding layer rise, such that silicon dioxide at the interface appropriately contracts to form an isolation layer with a relatively high density. In addition, in this invention, a hollow glass tube is used as a target rod, and the hollow glass tube which is the target rod is directly connected with the core layer loose body. During the subsequent dehydration, not only a dehydration atmosphere penetrates from the outside to the inside of the cladding layer loose body, but also the dehydration atmosphere directly enters the core layer through the hollow glass tube.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.