Glass ceramic with reduced lithium content
US11072557B2 · kind B2 · utility
Assignee
Inventors
Key dates
| Filing date | Dec 20, 2018 |
| Grant date | Jul 27, 2021 |
| Priority date | — |
| Expiry date | Dec 20, 2038 |
Classification
- Technology area (CPC F)Mechanical Engineering; Lighting; Heating
- CPC primaryF24C15/04
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
A transparent colored glass ceramic, in particular an LAS glass ceramic, suitable for use as a cooking surface is provided. The transparent colored glass ceramic includes high-quartz solid solution (HQ s.s.) as a main crystal phase and exhibits thermal expansion of −1 to +1 ppm/K in the range from 20° C. to 700° C. The glass ceramic has from 3.0 to 3.6 percent by weight of lithium oxide (Li2O) as constituents and either is colored with 0.003 to 0.05 percent by weight of vanadium oxide (V2O5) or is colored with 0.003 to 0.25 percent by weight of molybdenum oxide (MoO3).
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.