Patent · US Active

Three-dimensional composite material, preparation method thereof and application thereof in removal of water pollutants by visible light catalytic degrading

US11084027B2 · kind B2 · utility

0Cited by
0References
15Claims
0Family size

Assignee

Inventors

Key dates

Filing dateApr 26, 2019
Grant dateAug 10, 2021
Priority date
Expiry dateJan 2, 2040

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC02F2305/10
  • WIPO fieldChemical engineering
  • WIPO sectorChemistry

Abstract

A method of preparing a three-dimensional composite material includes the following steps: preparing polystyrene by soap-free emulsion polymerizing, obtaining polystyrene opal by a vertical deposition method, synthesizing MoP IO (molybdenum phosphide inverse opal), and compounding with quantum points CdS, so as to obtain a novel inorganic composite material, namely cadmium sulfide quantum dot-compounded MoP IO. The preparation method has the advantages that the MoP IO is prepared first, and the MoP IO is of a three-dimensional cyclic pore structure and has the photonic band gap feature, so that the MoP IO has better catalysis effect in light catalysis in comparison with that of common porous material; the MoP IO is compounded with the cadmium sulfide quantum dots, so that the light absorbing ability is enhanced, and the composite material capable of absorbing the visible light is obtained.