Rapid-hardening underground pipeline grouting repair polymer and preparing method

US11104612B2 · kind B2 · utility

0Cited by
3References
5Claims
0Family size

Assignee

Inventors

Key dates

Filing dateMay 18, 2019
Grant dateAug 31, 2021
Priority date
Expiry dateAug 1, 2039

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC04B2111/70
  • WIPO fieldMacromolecular chemistry, polymers
  • WIPO sectorChemistry

Abstract

The present invention provides a rapid-hardening underground pipeline grouting repair polymer and a preparing method thereof for underground pipes. The rapid-hardening underground pipeline grouting repair polymer comprises the base resin and the hardener, weight ratio of which is 2:1-1:1. The base resin comprises 50 to 160 parts by weight of an isocyanate; 20 to 100 parts of a chlorophosphate mixture with a density over 1400 kg/m3; a parts by weight ratio of the isocyanate and chlorophosphate is 1:1-4:1. The hardener comprises 30 to 60 parts by weight of a chlorophosphate mixture with a density over 1400 kg/m3, 5 to 15 parts of a propyl formate, a methyl propionate or a mixture of a propyl formate and a methyl propionate, 15 to 55 parts of a polyol, 1 to 3 parts of a surfactant, 2 to 6 parts of a catalyst, 0 to 0.5 parts of water and 0 to 1 parts of a colorant.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.