Abstract
The attenuation material composition disclosed in the present disclosure comprises a room temperature vulcanized silicone rubber, an epoxy resin, a first curing agent and a second curing agent, wherein the first curing agent comprises ethyl orthosilicate and dibutyltin oxide; and the weight ratio of the room temperature vulcanized silicone rubber to the epoxy resin is (0.1-1):1.