Corrosion resistive materials, systems, and methods of forming and using the materials and systems

US11124865B2 · kind B2 · utility

0Cited by
1References
14Claims
0Family size

Assignee

Inventors

Key dates

Filing dateAug 28, 2018
Grant dateSep 21, 2021
Priority date
Expiry dateJun 15, 2039

Classification

  • Technology area (CPC F)Mechanical Engineering; Lighting; Heating
  • CPC primaryF28F21/087
  • WIPO fieldThermal processes and apparatus
  • WIPO sectorMechanical engineering

Abstract

A method to reduce corrosion rates of materials at high temperatures may include heating a mixture and applying the heated mixture to a material to be rendered thermodynamically noble. The mixture may include carbon monoxide and carbon dioxide and the material rendered thermodynamically noble may include copper or other material having similar physical properties. The copper or other similar material may be applied to a structural material and provide a surface interfacing with the mixture of carbon monoxide and carbon dioxide to prevent corrosion of the structural material. In some cases, the structural material may form a heat exchanger defining passageways for a working fluid of a power system and/or may form other passageways of the power system. The copper may be applied to the passageways as a protective coating and then made thermodynamically noble at high temperatures after interactions with the mixture of carbon monoxide and carbon dioxide.