Patent · US Active

Composite positive active material, method of preparing the same, and lithium secondary battery including positive electrode including the same

US11133501B2 · kind B2 · utility

0Cited by
1References
13Claims
0Family size

Assignee

Inventors

Key dates

Filing dateOct 28, 2016
Grant dateSep 28, 2021
Priority date
Expiry dateMar 4, 2039

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY02E60/10
  • WIPO fieldElectrical machinery, apparatus, energy
  • WIPO sectorElectrical engineering

Abstract

A composite positive active material includes a lithium nickel cobalt aluminum composite oxide. A full width at half maximum (FWHM) of a peak of a (104) plane of the lithium nickel cobalt aluminum composite oxide is 0.15 or less and an FWHM of a peak of a (108) plane of the lithium nickel cobalt aluminum composite oxide is 0.15 or less, the peaks being obtained by X-ray diffraction analysis using a CuKα X-ray. A method of preparing the composite positive active material, and a lithium secondary battery including a positive electrode including the composite positive active material are disclosed.