High thermal stability melamine octamolybdate and use thereof as a smoke suppressant in polymer compositions
US11142630B2 · kind B2 · utility
Assignee
Inventors
Key dates
| Filing date | Sep 23, 2019 |
| Grant date | Oct 12, 2021 |
| Priority date | — |
| Expiry date | Sep 23, 2039 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC08K2003/2227
- WIPO fieldMacromolecular chemistry, polymers
- WIPO sectorChemistry
Abstract
Processes for producing melamine octamolybdates having high thermal stability include a step of reacting molybdenum trioxide and melamine in an acidic aqueous system at a pH of less than or equal to about 4 to form a slurry of the melamine octamolybdate. The resulting melamine octamolybdate can be characterized by a decomposition onset temperature (or a temperature at a weight loss of 1%, or a temperature at a weight loss of 2%) on a thermogravimetric analysis curve of greater than 300° C., and is useful in polymer compositions as a smoke suppressant.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.