Method and facility for manufacturing cross-linked fiberglass material
US11149366B2 · kind B2 · utility
Assignee
Inventors
Key dates
| Filing date | Jul 28, 2016 |
| Grant date | Oct 19, 2021 |
| Priority date | — |
| Expiry date | May 25, 2037 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY02P40/50
- WIPO fieldOther special machines
- WIPO sectorMechanical engineering
Abstract
The invention relates to a method and facility for manufacturing a cross-linked fiberglass material, in which melted glass is produced in a melting furnace heated via combustion of a fuel with an oxygen-rich oxidant. The melted glass is converted into glass filaments, the filaments are bonded, a sheet is made from the bonded filaments, and the sheet is then cross-linked. The fumes from the melting furnace are used to preheat a combustion reagent in two steps: a first step in which air is heated via heat exchange with the fumes, and a second step in which the combustion reagent is preheated via heat exchange with the hot air. The air is then used in the cross-linking step of the method for converting the melted glass into a fiberglass material.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.