Method for manufacturing powder magnetic core
US11192183B2 · kind B2 · utility
Assignee
Inventors
Key dates
| Filing date | Sep 16, 2016 |
| Grant date | Dec 7, 2021 |
| Priority date | — |
| Expiry date | Feb 13, 2039 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC22C2202/02
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
A powder magnetic core manufacturing method includes: a first step of mixing a binder with a soft magnetic material powder containing Fe-M (M: Al or Cr)-based alloy particles on which an insulating layer is formed; a second step of filling a pressing die with a mixture obtained through the first step, subjecting the mixture to pressing to obtain a green compact, and slidingly demolding the green compact from the pressing die; a third step of processing the green compact after the second step and removing expansion deformed matter of the alloy particles present in a region of pressing flaws formed on a surface of the green compact during the slidingly demolding; and a fourth step of subjecting the green compact after the third step to heat treatment to oxidize surfaces of the Fe-M (M: Al or Cr)-based alloy particles at high temperature, so that the oxide phase is formed.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.