Recovery of mining processing product using boronic acid-containing polymers

US11208332B2 · kind B2 · utility

1Cited by
90References
19Claims
0Family size

Assignee

Inventors

Key dates

Filing dateSep 30, 2019
Grant dateDec 28, 2021
Priority date
Expiry dateSep 30, 2039

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY02P10/20
  • WIPO fieldChemical engineering
  • WIPO sectorChemistry

Abstract

Methods and compositions for improving performance of flocculants in an industrial production process. Methods include pH triggered cross-linking reaction between a flocculating agent, such as dextran, and a composition comprising a boronic acid-containing polymer. The pH trigger can be provided by a fluid having a pH of 8 or more. The production process can be a Bayer Process and the fluid is caustic liquor or slurry in the fluid circuit of the Bayer, wherein the reaction time is reduced over conventional methods and the cross-linked dextran composition effectuates improved flocculation of the trihydrate particles.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.