Abstract

Mortar with small autogenous shrinkage strain and a method for producing the same are provided.Mortar has binder and fine aggregate, wherein the binder includes cement and fine mineral powder, and the mortar is formed by being mixed with water. The fine aggregate is air granulated ferronickel slag, and weight ratio of water to a combination of the binder and the fine aggregate is 7.0% or more and 9.0% or less. Such mortar can be produced by mixing binder, fine aggregate and water.