Rubber composition comprising a specific hydrocarbon resin
US11220591B2 · kind B2 · utility
Assignee
Inventors
Key dates
| Filing date | Dec 5, 2017 |
| Grant date | Jan 11, 2022 |
| Priority date | — |
| Expiry date | Feb 2, 2038 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC08L2312/00
- WIPO fieldMacromolecular chemistry, polymers
- WIPO sectorChemistry
Abstract
A rubber composition based on at least: from 50 to 100 phr of one or more diene elastomers, referred to as very low glass transition temperature (Tg) diene elastomers, having a Tg within a range of from −110° C. to −70° C., selected from butadiene homopolymers, copolymers of butadiene and of a vinylaromatic monomer, having a content of vinylaromatic units of between 0 and 5% by weight, and mixtures thereof a reinforcing filler a crosslinking system; and from 40 to 150 phr of at least one hydrogenated hydrocarbon resin predominantly composed of units derived from C9 monomers, the resin having a content of aromatic protons of less than 25% and a content of ethylenic protons of less than 1%.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.