Abstract

The invention relates to a method for producing rock wool and cast iron by melting a mixture of materials such as basalt, blast-furnace slag, coke and components necessary for melting, with an admixture containing alumina, said admixture making it possible to adjust the alumina content in order to obtain a rock wool having the following composition (as wt %): Al2O3: 18-22; SiO2: 40-50; CaO: 10-15; MgO: <10; FeO: <2; Na2O: <4; K2O: <2. The method includes the following operations: producing by melting a slag and a cast iron, separating the slag and the cast iron, and performing a fibring operation on the slag followed by a bonding operation in order to obtain the rock wool. According to the invention, at least one spent adsorbent and/or catalyst is used as an admixture, said catalyst containing alumina in Al2O3 form. Said adsorbent and/or catalyst preferably contains at least one metal, and said metal is retrieved in the cast iron.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.