Patent · US Active

Injection method for solid retarded acid

US11254859B2 · kind B2 · utility

0Cited by
1References
3Claims
0Family size

Assignee

Inventors

Key dates

Filing dateJul 22, 2020
Grant dateFeb 22, 2022
Priority date
Expiry dateJul 22, 2040

Classification

  • Technology area (CPC E)Fixed Constructions
  • CPC primaryE21B41/02
  • WIPO fieldBasic materials chemistry
  • WIPO sectorChemistry

Abstract

An injection method for a solid retarded acid includes mixing a solid acidic substance with a natural polymer, extruding through an extruder to produce particles; putting the produced particles in a coating pan, and sprinkling zinc acetate powder; turning on the coating pan to rotate while irradiating with an infrared lamp; spraying a glycolic acid aqueous solution with a spray gun, and continuing to rotate to obtain the solid retarded acid; injecting non-reactive liquid and the solid retarded acid into the a sand mixing truck; after the mixture is uniformly mixed in the sand mixing truck, injecting the mixture into a formation by a fracturing truck; conveying the solid retarded acid to a designated location, then stopping a pump, removing pipelines, and opening the well for gushing. The method is good in drag reduction, easy for flowback, thereby reducing the construction cost and facilitating environmental protection, and has broad application.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.