Patent · US Active

Delayed cracking prevention during drawing of high strength steel

US11254996B2 · kind B2 · utility

0Cited by
3References
13Claims
0Family size

Assignee

Inventors

Key dates

Filing dateJun 24, 2019
Grant dateFeb 22, 2022
Priority date
Expiry dateFeb 20, 2040

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC21D2211/001
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

This invention relates to prevention of delayed cracking of metal alloys during drawing which may occur from hydrogen attack. The alloys find applications in parts or components used in vehicles, such as bodies in white, vehicular frames, chassis, or panels.