Patent · US Active

Steel alloy and method for heat treating steel alloy components

US11286534B2 · kind B2 · utility

0Cited by
6References
23Claims
0Family size

Assignee

Inventors

Key dates

Filing dateJul 16, 2019
Grant dateMar 29, 2022
Priority date
Expiry dateFeb 16, 2040

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC22C38/52
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

A steel alloy including, by weight percent: Ni: 18 to 19%; Co: 11.5 to 12.5%; Mo: 4.6 to 5.2%; Ti: 1.3 to 1.6%; Al: 0.05 to 0.15%; Nb: 0.15 to 0.30%; B: 0.003 to 0.020%; Cr: max 0.25%; Mn: max 0.1%; Si: max 0.1%; C: max 0.03%; P: max 0.005%; and S: max 0.002%, the balance being iron plus incidental impurities.