Patent · US Active

Seamless steel pipe and method for producing the seamless steel pipe

US11313005B2 · kind B2 · utility

1Cited by
0References
28Claims
0Family size

Assignee

Inventors

Key dates

Filing dateMay 18, 2017
Grant dateApr 26, 2022
Priority date
Expiry dateJul 22, 2038

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC22C38/32
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

The seamless steel pipe of the present embodiment consists of in mass %, C: 0.21 to 0.35%, Si: 0.10 to 0.50%, Mn: 0.05 to 1.00%, P: 0.025% or less, S: 0.010% or less, Al: 0.005 to 0.100%, N: 0.010% or less, Cr: 0.05 to 1.50%, Mo: 0.10 to 1.50%, Nb: 0.010 to 0.050%, B: 0.0003 to 0.0050%, and Ti: 0.002 to 0.050%, the balance being Fe and impurities. In a main body region of the seamless steel pipe, a grain size number of prior-austenite grain conforming to ASTM E112 is 7.0 or more, a difference between a maximum value and a minimum value of the grain size number is 1.0 or less, yield strength is 655 to less than 862 MPa, and a difference between a maximum value and a minimum value of tensile strength is 27.6 MPa or less.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.