Multi-solid waste activated concrete with high-silicon iron ore tailings and preparation method thereof
US11325861B1 · kind B1 · utility
Assignee
Inventors
Key dates
| Filing date | Jan 4, 2022 |
| Grant date | May 10, 2022 |
| Priority date | — |
| Expiry date | Jan 4, 2042 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY02W30/91
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
Multi-solid waste activated concretes with high-silicon iron ore tailings and preparation methods thereof are disclosed. In at least some embodiments, the concrete is prepared from raw materials including 360-380 kg/m3 of a cement, 30-40 kg/m3 of fly ash, 30-40 kg/m3 of a modified ultrafine sand of high-silicon iron ore tailings, 930-950 kg/m3 of a waste stone of tailings, 870-930 kg/m3 of a fine sand of tailings, 160-170 kg/m3 of water, and 4-8 kg/m3 of an additive.