Microporous and hierarchical porous carbon
US11328878B2 · kind B2 · utility
Assignee
Inventors
Key dates
| Filing date | Jun 26, 2019 |
| Grant date | May 10, 2022 |
| Priority date | — |
| Expiry date | Nov 5, 2039 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY02E60/10
- WIPO fieldElectrical machinery, apparatus, energy
- WIPO sectorElectrical engineering
Abstract
A porous carbon material includes a hierarchical porous structure including a primary microporous structure and at least one of a secondary mesoporous structure and a secondary macroporous structure. The porous carbon material is formed by combining a halogenated-hydrocarbon, an aprotic hydrocarbon solvent, and a reductant to initiate a reaction that forms intermediate particles having a microporous framework; and subjecting the intermediate particles to a heat treatment at a heat treatment temperature ranging from about 300° C. to less than 1,500° C. for a heat treatment time period ranging from about 20 minutes to about 10 hours to thereby form the porous carbon material. The aprotic hydrocarbon solvent is selected from the group consisting of toluene, hexane, cyclohexane, and combinations thereof.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.