LCM composition with controlled viscosity and cure time and methods of treating a lost circulation zone of a wellbore

US11332656B2 · kind B2 · utility

2Cited by
63References
20Claims
0Family size

Assignee

Inventors

Key dates

Filing dateDec 18, 2019
Grant dateMay 17, 2022
Priority date
Expiry dateDec 18, 2039

Classification

  • Technology area (CPC E)Fixed Constructions
  • CPC primaryE21B33/138
  • WIPO fieldBasic materials chemistry
  • WIPO sectorChemistry

Abstract

A lost circulation material (LCM) composition for sealing lost circulation zones in wellbores may include 50 weight percent to 97 weight percent epoxy resin, 2 weight percent to 30 weight percent curing agent, 0.1 weight percent to 40 weight percent weighting material, and 0.1 weight percent to 20 weight percent amide accelerator. The LCM composition may have a density of greater than or equal to 1121 kilograms per cubic meter and may be capable of being injected through a drill bit of a drill string into the lost circulation zone. The amide accelerator may enable the viscosity of the LCM composition to be reduced while providing a reduced cure time. The LCM compositions are suitable for treating high-injectivity lost circulation zones.