Patent · US Active

Method of manufacturing hot-press-formed steel member

US11344941B2 · kind B2 · utility

0Cited by
1References
17Claims
0Family size

Assignee

Inventors

Key dates

Filing dateJul 18, 2012
Grant dateMay 31, 2022
Priority date
Expiry dateJun 9, 2034

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC21D2211/008
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

In a method for obtaining a hot-press-formed steel member, a steel sheet containing 0.10-0.30 mass % of C, 1.0-2.5 mass % of Si, 1.0-3.0 mass % of Si and Al in total, and 1.5-3.0 mass % of Mn is heated at a heating temperature of not less than the Ac3 transformation point. The steel sheet is hot-press formed for one or more times. The starting temperature of the hot pressing is not more than the heating temperature but not less than the Ms point. The average cooling rate from (Ms point−150)° C. to 40° C. is 5° C./s or less. The hot-press-formed steel member has high strength, high tensile elongation, high bendability, excellent deformation characteristics at the time of collision crush, and excellent delayed fracture resistance.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.