Ultra-thin Ni—Fe-MOF nanosheet, preparation method and use thereof

US11396521B2 · kind B2 · utility

1Cited by
0References
3Claims
0Family size

Assignee

Inventors

Key dates

Filing dateNov 7, 2018
Grant dateJul 26, 2022
Priority date
Expiry dateNov 7, 2038

Classification

  • Technology area (CPC B)Performing Operations; Transporting
  • CPC primaryB82Y40/00
  • WIPO fieldSurface technology, coating
  • WIPO sectorChemistry

Abstract

The present invention discloses a method for preparing an ultra-thin Ni—Fe-MOF nanosheet, which comprises the steps of dissolving an organic ligand in an organic solvent, dripping the resulting solution to an aqueous solution containing a nickel salt and an iron salt, mixing uniformly and reacting at 140-160° C. for 3-6 h to obtain the ultra-thin Ni—Fe-MOF nanosheet, wherein the organic ligand is terephthalic acid and/or disodium terephthalate, and the organic solvent is N,N-dimethylacetamide and/or N,N-dimethylformamide. The present invention discloses an ultra-thin Ni—Fe-MOF nanosheet, and use thereof. The preparation method does not require a surfactant, the surface of the product is neat and easy to be cleaned, and the large-scale synthesis of 2D ultra-thin MOF materials can be realized.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.