Patent · US Active

Tarnish and sweat resistant low karat gold alloys

US11401581B1 · kind B1 · utility

0Cited by
3References
4Claims
0Family size

Assignee

Inventors

Key dates

Filing dateJan 7, 2020
Grant dateAug 2, 2022
Priority date
Expiry dateAug 7, 2040

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC22F1/08
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

This invention provides low karat, low silver, 6 kt gold-copper-zinc alloys with acceptable workability that can be processed into wire, tube, sheet stock, or cast. The alloys are annealed at 1200° F., rapidly cooled, and heat treated at about 6000 to 800° F., which increases the hardness and durability in finished parts made from these alloys. The alloys include grain refiners. The alloys are resistant to oxidation from sweat and tarnishing. Additional fabrication operations can form jewelry items such as balls, chain, hoops and studs.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.