Method for controlled preparation of low molecular weight cellulose ether

US11407842B2 · kind B2 · utility

0Cited by
5References
13Claims
0Family size

Assignee

Inventors

Key dates

Filing dateJun 29, 2018
Grant dateAug 9, 2022
Priority date
Expiry dateJun 29, 2038

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC08L1/284
  • WIPO fieldMacromolecular chemistry, polymers
  • WIPO sectorChemistry

Abstract

A process includes: (a) providing an initial cellulose ether powder containing 0.5 to 10 weight-percent water based on total cellulose ether powder weight; (b) heating the initial cellulose ether powder to a temperature in a range of 30 to 130 degrees Celsius; (c) before, during and/or after heating in step (b), adding solid base to the cellulose ether powder and mixing with the initial cellulose ether powder to form a cellulose ether/base mixture; (d) adding volatile acid to the cellulose ether/base mixture and mixing; and (e) allowing the volatile acid to hydrolyze the initial cellulose ether to form a final cellulose ether having a lower viscosity than the initial cellulose ether.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.