All-steel fitting
US11414792B2 · kind B2 · utility
Assignee
Inventors
Key dates
| Filing date | May 5, 2015 |
| Grant date | Aug 16, 2022 |
| Priority date | — |
| Expiry date | Apr 4, 2036 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY02P10/25
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
In the method according to the invention, a wire (11) provided with teeth (15) passes sequentially through a first inductor (16) and a second inductor (18). The inductors (16, 18) function at different frequencies and generate different temperatures. The first inductor (16) heats in particular the base section (17), which is not to be hardened, to a high temperature below the austenitizing temperature range. The second inductor (18) heats the teeth (15) to a still higher second temperature within the austenitizing temperature range. Defined, hardened teeth of consistently high quality result at quenching.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.