Method for manufacture of transition metal oxide fine particles

US11420258B2 · kind B2 · utility

0Cited by
1References
19Claims
0Family size

Assignee

Inventors

Key dates

Filing dateMay 10, 2019
Grant dateAug 23, 2022
Priority date
Expiry dateMay 16, 2039

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC01P2006/80
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

The present invention provides a method for the manufacture of transition metal oxide fine particles, the method comprising the steps of: heating a strong-alkaline aqueous solution while stirring same; adding to and dissolving in the heated strong-alkaline aqueous solution a transition metal oxide; adding a strong-acid aqueous solution to the strong alkaline aqueous solution in which the transition metal oxide is dissolved, while stirring same, thereby re-dissolving a solid generated at the interface between the strong-alkaline aqueous solution and the strong-acid aqueous solution; adjusting the pH of the mixed aqueous solution resulting from mixing the strong-alkaline aqueous solution and the strong acid aqueous solution, through adjustment of the adding rate and amount of the strong-acid aqueous solution, to precipitate transition metal oxide fine particles; and separating the transition metal oxide fine particles from the mixed aqueous solution and sequentially washing, drying, and thermally treating the separated transition metal oxide fine particles.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.