Abstract
A method for producing a foamed particle molded article provided with a skin, includes: forming a hollow molded article; filling a hollow part of the hollow molded article with polypropylene-based resin foamed particles; and heating and fusing the particles to each other. A melt elongation at 190° C. of the polypropylene-based resin forming the hollow molded article is 100 m/min or more. A half-crystallization time at 100° C. of the polypropylene-based resin is between 25 to 80 seconds. In heat flux differential scanning calorimetry, a melting peak temperature of the polypropylene-based resin is between 130 to 155° C., a partial heat of fusion at 140° C. or more of the polypropylene-based resin is between 20 to 50 J/g, and a ratio of the partial heat of fusion of the polypropylene-based resin to the total (partial heat of fusion/total heat of fusion) is between 0.2 to 0.8.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.