Abstract
A method for the fabrication of a hot rolled steel includes providing a liquid metal comprising a certain chemical composition; carrying out a vacuum or SiCa treatment, the chemical composition including, expressed by weight 0.0005%≤Ca≤0.005%, if a SiCA treatment is carried out; dissolving quantities of Ti and N in the liquid metal so as to satisfy (% [Ti])×(% [N])<6.10−4%2; casting the steel to obtain a cast semi-finished product; rolling the cast semi-finished product with an end-of-rolling temperature between 880° C. and 930° C., a reduction rate of the penultimate pass being less than 0.25, and a start-of-rolling temperature of the penultimate pass being less than 960° C. to obtain a hot-rolled product, then cooling the hot rolled product at a rate between 20 and 150° C./s to obtain a hot rolled steel sheet; and coiling the hot rolled product to obtain a hot rolled steel sheet.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.