Heat treatments for improved ductility of Ni—Cr—Co—Mo—Ti—Al alloys

US11453939B2 · kind B2 · utility

1Cited by
1References
17Claims
0Family size

Assignee

Inventor

Key dates

Filing dateNov 9, 2018
Grant dateSep 27, 2022
Priority date
Expiry dateFeb 26, 2039

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC22C2202/00
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

In a method for heat treating alloy compositions within UNS N07028 the alloy composition is heated at a temperature between 1550° F. and 1750° F. for at least two hours, and then heated at a lower temperature between 1300° F. and 1550° F. for at least two hours. The alloy composition may be heated at a temperature between 1850° F. and 1950° F. for at least one hour before heating the alloy composition at a temperature between 1550° F. and 1750° F.