A flat glass is provided that exhibits high transmittance to electromagnetic radiation in a range of wavelengths from 200 nm to 1500 nm. The transmittance for the flat glass having a thickness of 1 mm is 20% or more at a wavelength of 254 nm, 82% or more at a wavelength of 300 nm, 90% or more at a wavelength of 350 nm, 92% or more at a wavelength of 546 nm, 92.5% or more at a wavelength of 1400 nm, 91.5% or more in a wavelength range from 380 nm to 780 nm, and 92.5% or more in a wavelength range from 780 nm to 1500 nm.