Abstract
The present invention discloses a method for detoxifying chromium slag by using high sulfur coal. The method includes: sieving chromium slag into coarse-grained chromium slag and fine-grained chromium slag, air-drying and crushing both the coarse-grained chromium slag and the fine-grained chromium slag; separately mixing the crushed coarse-grained chromium slag and fine-grained chromium slag with the crushed high sulfur coal uniformly; adjusting pH values of a coarse-grained slag mixture and a fine-grained slag mixture to 8.0-11.0 and moisture content thereof to 12%-18%; conducting reduction on the treated coarse-grained slag mixture and fine-grained slag mixture, where the reduction temperature of the fine-grained slag mixture is 500-700° C., the reduction time of the fine-grained slag mixture is 10-30 min, the reduction temperature of the coarse-grained slag mixture is 800-1000° C., the reduction time of the coarse-grained slag mixture is 10-30 min; after the reduction, conducting water quenching, and discharging the product.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.