Patent · US Active

Rubber composition comprising a specific hydrocarbon resin

US11492465B2 · kind B2 · utility

1Cited by
17References
20Claims
0Family size

Assignee

Inventors

Key dates

Filing dateApr 13, 2018
Grant dateNov 8, 2022
Priority date
Expiry dateApr 13, 2038

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC08L2312/00
  • WIPO fieldMacromolecular chemistry, polymers
  • WIPO sectorChemistry

Abstract

A rubber composition is based on at least: from 60 to 100 phr of one or more diene elastomers, referred to as very low glass transition temperature (Tg) diene elastomers, exhibiting a Tg within a range extending from −110° C. to −70° C., chosen from butadiene homopolymers, copolymers of butadiene and of vinylaromatic monomer, exhibiting a content of vinylaromatic unit of between 0% and 5% by weight, and the mixtures of these; a reinforcing filler; crosslinking system; and from 50 to 150 phr of at least one hydrocarbon resin predominantly composed of units resulting from α-pinene monomers, the resin exhibiting an aliphatic proton content of greater than 95%.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.