Sintered lithium cobaltite electrodes
US11505501B1 · kind B1 · utility
Assignee
Inventors
Key dates
| Filing date | Aug 20, 2021 |
| Grant date | Nov 22, 2022 |
| Priority date | — |
| Expiry date | Aug 20, 2041 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY02E60/10
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
A method for forming a sintered composition including providing a slurry precursor including a lithium-, sodium-, or magnesium-based compound; tape casting the slurry precursor to form a green tape; and sintering the green tape at a temperature in a range of 500° C. to 1350° C. for a time in a range of less than 60 min to form a sintered composition, such that the slurry precursor further includes a solvent and dispersant. The dispersant may include an amine compound, a carboxylic acid compound, or combinations, mixtures, or salts thereof.