Patent · US Active

Ultra-high molecular weight, ultra-fine particle size polyethylene, preparation method therefor and use thereof

US11530281B2 · kind B2 · utility

0Cited by
0References
15Claims
0Family size

Assignee

Inventors

Key dates

Filing dateFeb 19, 2019
Grant dateDec 20, 2022
Priority date
Expiry dateAug 11, 2040

Classification

  • Technology area (CPC F)Mechanical Engineering; Lighting; Heating
  • CPC primaryF16L9/12
  • WIPO fieldOther special machines
  • WIPO sectorMechanical engineering

Abstract

An ultra-high molecular weight, ultra-fine particle size polyethylene has a viscosity average molecular weight (Mv) greater than 1×106. The polyethylene is spherical or are sphere-like particles having a mean particle size of 10-100 μm, having a standard deviation of 2-15 μm and a bulk density of 0.1-0.3 g/mL. Using the polyethylene as a basic polyethylene, a grafted polyethylene can be obtained by means of a solid-phase grafting method; and a glass fiber-reinforced polyethylene composition comprising the polyethylene and glass fibers, and a sheet or pipe prepared therefrom; a solubilized ultra-high molecular weight, ultra-fine particle size polyethylene; and a fiber and a film prepared from the solubilized ultra-high molecular weight, ultra-fine particle size polyethylene may also be obtained. The method has simple steps, is easy to control, has a relatively low cost and a high repeatability, and can realize industrialisation.