Patent · US Active

Sintered friction material

US11534829B2 · kind B2 · utility

0Cited by
1References
4Claims
0Family size

Assignees

Inventors

Key dates

Filing dateApr 7, 2017
Grant dateDec 27, 2022
Priority date
Expiry dateAug 12, 2037

Classification

  • Technology area (CPC B)Performing Operations; Transporting
  • CPC primaryB22F2998/10
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

A sintered friction material is formed by pressure sintering mixed powder at 800° C. or above, the mixed powder consisting of, in mass %, Cu and/or Cu alloy: 40.0 to 80.0%, Ni: 0% or more and less than 5.0%, Sn: 0 to 10.0%, Zn: 0 to 10.0%, VC: 0.5 to 5.0%, Fe and/or Fe alloy: 2.0 to 40.0%, lubricant: 5.0 to 30.0%, metal oxide and/or metal nitride: 1.5 to 30.0%, and the balance being impurity.