Patent · US Active

Heat-resistant sintered material having excellent high-temperature wear resistance and salt damage resistance and method for producing same

US11578393B2 · kind B2 · utility

0Cited by
1References
6Claims
0Family size

Assignee

Inventors

Key dates

Filing dateMar 26, 2018
Grant dateFeb 14, 2023
Priority date
Expiry dateOct 5, 2039

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC21D2211/004
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

This heat-resistant sintered material has, as an overall composition, a composition including, in terms of % by mass, Cr: 15% to 30%, Ni: 8% to 30%, Si: 2.0% to 6.0%, and C: 0.5% to 2.5% with a remainder being Fe and inevitable impurities, wherein the heat-resistant sintered material has a structure in which hard phases are dispersed in a matrix, the matrix includes Fe, Cr, Ni, and Si, the hard phase includes Fe, Cr, and C, and a porosity is 2.0% or less.