Patent · US Active

Sintered body and method for manufacturing thereof

US11594756B2 · kind B2 · utility

0Cited by
0References
14Claims
0Family size

Assignee

Inventors

Key dates

Filing dateJul 28, 2020
Grant dateFeb 28, 2023
Priority date
Expiry dateMay 19, 2041

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY02E60/10
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

The sintered body has an average particle size in the range of 0.1 μm or more and 5 μm or less, includes gamet-type oxide base material particles having at least Li, La, and Zr, has 8% by volume or more of voids, and has an ionic conductivity of 1.0×10−5 S/cm or more at temperature of 25° C.