Delamination resistant glass containers with heat-tolerant coatings

US11608290B2 · kind B2 · utility

0Cited by
190References
29Claims
0Family size

Assignee

Inventors

Key dates

Filing dateMar 17, 2019
Grant dateMar 21, 2023
Priority date
Expiry dateSep 29, 2040

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY10T428/131
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

Disclosed herein are delamination resistant glass pharmaceutical containers which may include a glass body having a Class HGA1 hydrolytic resistance when tested according to the ISO 720:1985 testing standard. The glass body may have an interior surface and an exterior surface. The interior surface of the glass body does not comprise a boron-rich layer when the glass body is in an as-formed condition. A heat-tolerant coating may be bonded to at least a portion of the exterior surface of the glass body. The heat-tolerant coating may have a coefficient of friction of less than about 0.7 and is thermally stable at a temperature of at least 250° C. for 30 minutes.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.