Patent · US Active

Method for improving both strength and ductility of a press-hardening steel

US11613789B2 · kind B2 · utility

0Cited by
67References
18Claims
0Family size

Assignee

Inventors

Key dates

Filing dateMay 24, 2018
Grant dateMar 28, 2023
Priority date
Expiry dateAug 11, 2038

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC21D2211/008
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

A method of forming a shaped steel object, includes cutting a blank from an alloy composition. The alloy composition includes 0.1-1 wt. % carbon, 0.1-3 wt. % manganese, 0.1-3 wt. % silicon, 1-10 wt. % aluminum, and a balance being iron. The method also includes heating the blank to a temperature above a temperature at which austenite begins to form to generate a heated blank, transferring the heated blank to a die, forming the heated blank into a predetermined shape defined by the die to generate a shaped steel object, and decreasing the temperature of the shaped steel object to ambient temperature. The heating is performed under an atmosphere comprising at least one of an inert gas, a carbon (C)-based gas, and nitrogen (N2) gas.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.